Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 20 % Show Material materials with Dehnung A50 of 20 % |
Flächenreduzierung | 23.0 °C | 38 % Show Material materials with Flächenreduzierung of 38 % |
Kerbschlagenergie | 23.0 °C | 20 J Show Material materials with Kerbschlagenergie of 20 J |
Streckgrenze Rp 0,2 | 23.0 °C | 250 MPa Show Material materials with Streckgrenze Rp 0,2 of 250 MPa |
Zugfestigkeit | 23.0 °C | 485 - 655 MPa Show Material materials with Zugfestigkeit of 485 - 655 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.25 % Show Material materials with Chrom of 0.25 % |
Kohlenstoff | 0.35 % Show Material materials with Kohlenstoff of 0.35 % |
Mangan | 0.4 - 0.9 % Show Material materials with Mangan of 0.4 - 0.9 % |
Molybdän | 0.1 % Show Material materials with Molybdän of 0.1 % |
Nickel | 0.4 % Show Material materials with Nickel of 0.4 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.35 % Show Material materials with Silizium of 0.35 % |
Vanadium | 0.05 % Show Material materials with Vanadium of 0.05 % |