Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 18 % Show Material materials with Dehnung A50 of 18 % |
Flächenreduzierung | 20.0 °C | 38 % Show Material materials with Flächenreduzierung of 38 % |
Kerbschlagenergie | 20.0 °C | 41 J Show Material materials with Kerbschlagenergie of 41 J |
Yield Strength Rp0.2, short transverse | 20.0 °C | 345 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 345 MPa |
Zugfestigkeit | 20.0 °C | 550 - 725 MPa Show Material materials with Zugfestigkeit of 550 - 725 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.25 - 0.45 % Show Material materials with Chrom of 0.25 - 0.45 % |
Kohlenstoff | 0.27 % Show Material materials with Kohlenstoff of 0.27 % |
Mangan | 0.5 - 0.9 % Show Material materials with Mangan of 0.5 - 0.9 % |
Molybdän | 0.55 - 0.7 % Show Material materials with Molybdän of 0.55 - 0.7 % |
Nickel | 0.5 - 1 % Show Material materials with Nickel of 0.5 - 1 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.35 % Show Material materials with Silizium of 0.35 % |
Vanadium | 0.05 % Show Material materials with Vanadium of 0.05 % |