Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Nickel Molybdenum Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 12 % Show Material materials with Dehnung of 12 % | |
Elastizitätsmodul | 20.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Molybdenum Steel |
Flächenreduzierung | 20.0 °C | 36 % Show Material materials with Flächenreduzierung of 36 % | |
Kerbschlagenergie | 20.0 °C | 60 J Show Material materials with Kerbschlagenergie of 60 J | |
Poissonzahl | 20.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Molybdenum Steel |
Yield Strength Rp0.2, short transverse | 20.0 °C | 1100 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 1100 MPa | |
Zugfestigkeit | 20.0 °C | 1210 MPa Show Material materials with Zugfestigkeit of 1210 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 9E-6 - 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9E-6 - 1.3E-5 1/K | Typical for Nickel Molybdenum Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Nickel Molybdenum Steel | |
Wärmeleitfähigkeit | 20.0 °C | 44 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 44 W/(m·K) | Typical for Nickel Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 1.4 - 1.65 % Show Material materials with Chrom of 1.4 - 1.65 % |
Kohlenstoff | 0.23 - 0.28 % Show Material materials with Kohlenstoff of 0.23 - 0.28 % |
Mangan | 0.2 % Show Material materials with Mangan of 0.2 % |
Molybdän | 0.8 - 1 % Show Material materials with Molybdän of 0.8 - 1 % |
Nickel | 2.75 - 3.25 % Show Material materials with Nickel of 2.75 - 3.25 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |