Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 13 % Show Material materials with Dehnung of 13 % |
Flächenreduzierung | 20.0 °C | 40 % Show Material materials with Flächenreduzierung of 40 % |
Kerbschlagenergie | 20.0 °C | 70 J Show Material materials with Kerbschlagenergie of 70 J |
Yield Strength Rp0.2, short transverse | 20.0 °C | 965 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 965 MPa |
Zugfestigkeit | 20.0 °C | 1035 MPa Show Material materials with Zugfestigkeit of 1035 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.4 - 0.7 % Show Material materials with Chrom of 0.4 - 0.7 % |
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % |
Mangan | 0.6 - 0.9 % Show Material materials with Mangan of 0.6 - 0.9 % |
Molybdän | 0.3 - 0.65 % Show Material materials with Molybdän of 0.3 - 0.65 % |
Nickel | 4.75 - 5.25 % Show Material materials with Nickel of 4.75 - 5.25 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.2 - 0.35 % Show Material materials with Silizium of 0.2 - 0.35 % |
Vanadium | 0.05 - 0.1 % Show Material materials with Vanadium of 0.05 - 0.1 % |