Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 6 % Show Material materials with Dehnung of 6 % |
Flächenreduzierung | 20.0 °C | 25 % Show Material materials with Flächenreduzierung of 25 % |
Kerbschlagenergie | 20.0 °C | 20 J Show Material materials with Kerbschlagenergie of 20 J |
Yield Strength Rp0.2, short transverse | 20.0 °C | 1550 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 1550 MPa |
Zugfestigkeit | 20.0 °C | 1720 MPa Show Material materials with Zugfestigkeit of 1720 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 1.9 - 2.25 % Show Material materials with Chrom of 1.9 - 2.25 % |
Kohlenstoff | 0.41 - 0.46 % Show Material materials with Kohlenstoff of 0.41 - 0.46 % |
Mangan | 0.75 - 1 % Show Material materials with Mangan of 0.75 - 1 % |
Molybdän | 0.45 - 0.6 % Show Material materials with Molybdän of 0.45 - 0.6 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 1.4 - 1.75 % Show Material materials with Silizium of 1.4 - 1.75 % |
Vanadium | 0.03 - 0.08 % Show Material materials with Vanadium of 0.03 - 0.08 % |