Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Dichte of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 10 - 12 % Show Material materials with Dehnung of 10 - 12 % | |
Elastizitätsmodul | 20.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | Typical for Martensitic Stainless Steel |
Flächenreduzierung | 20.0 °C | 40 - 45 % Show Material materials with Flächenreduzierung of 40 - 45 % | |
Poissonzahl | 20.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Martensitic Stainless Steel |
Yield Strength Rp0.2, short transverse | 20.0 °C | 965 - 1100 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 965 - 1100 MPa | |
Zugfestigkeit | 20.0 °C | 1210 - 1520 MPa Show Material materials with Zugfestigkeit of 1210 - 1520 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Schmelzpunkt | 1375 - 1450 °C Show Material materials with Schmelzpunkt of 1375 - 1450 °C | Typical for Martensitic Stainless Steel | |
Spezifische Wärmekapazität | 20.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Wärmeleitfähigkeit | 20.0 °C | 14 - 31 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 20.0 °C | 6E-7 Ω·m Show Material materials with spezifischer Widerstand of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Chrom | 11 - 12.5 % Show Material materials with Chrom of 11 - 12.5 % |
Kobalt | 0.25 % Show Material materials with Kobalt of 0.25 % |
Kohlenstoff | 0.2 - 0.25 % Show Material materials with Kohlenstoff of 0.2 - 0.25 % |
Mangan | 0.5 - 1 % Show Material materials with Mangan of 0.5 - 1 % |
Molybdän | 0.9 - 1.25 % Show Material materials with Molybdän of 0.9 - 1.25 % |
Nickel | 0.5 - 1 % Show Material materials with Nickel of 0.5 - 1 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Titan | 0.05 % Show Material materials with Titan of 0.05 % |
Vanadium | 0.2 - 0.3 % Show Material materials with Vanadium of 0.2 - 0.3 % |
Wolfram | 0.9 - 1.25 % Show Material materials with Wolfram of 0.9 - 1.25 % |
Zinn | 0.04 % Show Material materials with Zinn of 0.04 % |