Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 8 - 12 % Show Material materials with Dehnung of 8 - 12 % |
Flächenreduzierung | 20.0 °C | 40 - 50 % Show Material materials with Flächenreduzierung of 40 - 50 % |
Kerbschlagenergie | 20.0 °C | 35 J Show Material materials with Kerbschlagenergie of 35 J |
Yield Strength Rp0.2, short transverse | 20.0 °C | 965 - 1240 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 965 - 1240 MPa |
Zugfestigkeit | 20.0 °C | 1140 - 1380 MPa Show Material materials with Zugfestigkeit of 1140 - 1380 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 15.5 - 17.5 % Show Material materials with Chrom of 15.5 - 17.5 % |
Kohlenstoff | 0.07 % Show Material materials with Kohlenstoff of 0.07 % |
Kupfer | 3 - 5 % Show Material materials with Kupfer of 3 - 5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 3 - 5 % Show Material materials with Nickel of 3 - 5 % |
Niobium | 0.15 - 0.45 % Show Material materials with Niobium of 0.15 - 0.45 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |