Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 6 % Show Material materials with Dehnung of 6 % |
Flächenreduzierung | 20.0 °C | 25 % Show Material materials with Flächenreduzierung of 25 % |
Yield Strength Rp0.2, short transverse | 20.0 °C | 965 - 1100 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 965 - 1100 MPa |
Zugfestigkeit | 20.0 °C | 1140 - 1240 MPa Show Material materials with Zugfestigkeit of 1140 - 1240 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.75 - 1.5 % Show Material materials with Aluminium of 0.75 - 1.5 % |
Chrom | 16 - 18 % Show Material materials with Chrom of 16 - 18 % |
Kohlenstoff | 0.09 % Show Material materials with Kohlenstoff of 0.09 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 6.5 - 7.75 % Show Material materials with Nickel of 6.5 - 7.75 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |