Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 10 - 12 % Show Material materials with Dehnung of 10 - 12 % |
Flächenreduzierung | 20.0 °C | 25 % Show Material materials with Flächenreduzierung of 25 % |
Kerbschlagenergie | 20.0 °C | 20 J Show Material materials with Kerbschlagenergie of 20 J |
Yield Strength Rp0.2, short transverse | 20.0 °C | 965 - 1240 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 965 - 1240 MPa |
Zugfestigkeit | 20.0 °C | 1140 - 1450 MPa Show Material materials with Zugfestigkeit of 1140 - 1450 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 15 - 16 % Show Material materials with Chrom of 15 - 16 % |
Kohlenstoff | 0.1 - 0.15 % Show Material materials with Kohlenstoff of 0.1 - 0.15 % |
Mangan | 0.5 - 1.25 % Show Material materials with Mangan of 0.5 - 1.25 % |
Molybdän | 2.5 - 3.25 % Show Material materials with Molybdän of 2.5 - 3.25 % |
Nickel | 4 - 5 % Show Material materials with Nickel of 4 - 5 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Stickstoff | 0.07 - 0.13 % Show Material materials with Stickstoff of 0.07 - 0.13 % |