Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 12 % Show Material materials with Dehnung of 12 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 55 % Show Material materials with Flächenreduzierung of 55 % | |
Kerbschlagenergie | 23.0 °C | 45 J Show Material materials with Kerbschlagenergie of 45 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 1380 MPa Show Material materials with Streckgrenze Rp 0,2 of 1380 MPa | |
Zugfestigkeit | 23.0 °C | 1450 MPa Show Material materials with Zugfestigkeit of 1450 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 - 0.15 % Show Material materials with Aluminium of 0.05 - 0.15 % |
Kobalt | 8 - 9 % Show Material materials with Kobalt of 8 - 9 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % |
Molybdän | 3 - 3.5 % Show Material materials with Molybdän of 3 - 3.5 % |
Nickel | 17 - 19 % Show Material materials with Nickel of 17 - 19 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Titan | 0.15 - 0.25 % Show Material materials with Titan of 0.15 - 0.25 % |