Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 13 % Show Material materials with Dehnung of 13 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 45 % Show Material materials with Flächenreduzierung of 45 % | |
Kerbschlagenergie | 23.0 °C | 35 J Show Material materials with Kerbschlagenergie of 35 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 1240 MPa Show Material materials with Streckgrenze Rp 0,2 of 1240 MPa | |
Zugfestigkeit | 23.0 °C | 1310 MPa Show Material materials with Zugfestigkeit of 1310 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.35 - 0.6 % Show Material materials with Chrom of 0.35 - 0.6 % |
Kobalt | 3.5 - 4.5 % Show Material materials with Kobalt of 3.5 - 4.5 % |
Kohlenstoff | 0.24 - 0.3 % Show Material materials with Kohlenstoff of 0.24 - 0.3 % |
Mangan | 0.1 - 0.35 % Show Material materials with Mangan of 0.1 - 0.35 % |
Molybdän | 0.35 - 0.6 % Show Material materials with Molybdän of 0.35 - 0.6 % |
Nickel | 7 - 9 % Show Material materials with Nickel of 7 - 9 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Vanadium | 0.06 - 0.12 % Show Material materials with Vanadium of 0.06 - 0.12 % |