Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.85 g/cm³ Show Material materials with Dichte of 7.85 g/cm³ | Typical for Carbon Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 20.0 °C | 22 - 23 % Show Material materials with Dehnung A50 of 22 - 23 % | |
Flächenreduzierung | 20.0 °C | 34 - 36 % Show Material materials with Flächenreduzierung of 34 - 36 % | |
Härte, Brinell | 20.0 °C | 137 - 183 [-] Show Material materials with Härte, Brinell of 137 - 183 [-] | |
Poissonzahl | 20.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Carbon Steel |
Schubmodule | 20.0 °C | 75 - 80 GPa Show Material materials with Schubmodule of 75 - 80 GPa | Typical for Carbon Steel |
Streckgrenze | 20.0 °C | 230 MPa Show Material materials with Streckgrenze of 230 MPa | |
Zugfestigkeit | 20.0 °C | 455 MPa Show Material materials with Zugfestigkeit of 455 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-5 1/K | Typical for Carbon Steel |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1425 - 1540 °C Show Material materials with Schmelzpunkt of 1425 - 1540 °C | Typical for Carbon Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 20.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |