Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 22 - 25 % Show Material materials with Dehnung A50 of 22 - 25 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 35 - 40 % Show Material materials with Flächenreduzierung of 35 - 40 % | |
Härte, Brinell | 23.0 °C | 174 - 217 [-] Show Material materials with Härte, Brinell of 174 - 217 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 295 - 305 MPa Show Material materials with Streckgrenze of 295 - 305 MPa | |
Zugfestigkeit | 23.0 °C | 570 - 585 MPa Show Material materials with Zugfestigkeit of 570 - 585 MPa |