Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 22 - 24 % Show Material materials with Dehnung A50 of 22 - 24 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 38 - 40 % Show Material materials with Flächenreduzierung of 38 - 40 % | |
Härte, Brinell | 23.0 °C | 163 - 207 [-] Show Material materials with Härte, Brinell of 163 - 207 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 345 MPa Show Material materials with Streckgrenze of 345 MPa | |
Zugfestigkeit | 23.0 °C | 550 MPa Show Material materials with Zugfestigkeit of 550 MPa |