Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 10 % Show Material materials with Dehnung A50 of 10 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 40 % Show Material materials with Flächenreduzierung of 40 % | |
Härte, Brinell | 23.0 °C | 331 [-] Show Material materials with Härte, Brinell of 331 [-] | |
Härte, Rockwell C | 23.0 °C | 35 [-] Show Material materials with Härte, Rockwell C of 35 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 1035 MPa Show Material materials with Streckgrenze of 1035 MPa | |
Zugfestigkeit | 23.0 °C | 1170 MPa Show Material materials with Zugfestigkeit of 1170 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.4 % Show Material materials with Aluminium of 0.4 % |
Chrom | 16 - 17.5 % Show Material materials with Chrom of 16 - 17.5 % |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 6 - 7.5 % Show Material materials with Nickel of 6 - 7.5 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Titan | 0.4 - 1.2 % Show Material materials with Titan of 0.4 - 1.2 % |