Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Härte, Brinell | 23.0 °C | 255 [-] Show Material materials with Härte, Brinell of 255 [-] | |
Härte, Rockwell B | 23.0 °C | 100 [-] Show Material materials with Härte, Rockwell B of 100 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 16 - 18 % Show Material materials with Chrom of 16 - 18 % |
Kohlenstoff | 0.95 - 1.2 % Show Material materials with Kohlenstoff of 0.95 - 1.2 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 0.4 - 0.8 % Show Material materials with Molybdän of 0.4 - 0.8 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Sauerstoff | 2E-3 % Show Material materials with Sauerstoff of 2E-3 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |