Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 10 % Show Material materials with Dehnung A50 of 10 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Elongation A200 | 23.0 °C | 8 % Show Material materials with Elongation A200 of 8 % | |
Härte, Brinell | 23.0 °C | 269 [-] Show Material materials with Härte, Brinell of 269 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 690 MPa Show Material materials with Streckgrenze of 690 MPa | |
Zugfestigkeit | 23.0 °C | 860 MPa Show Material materials with Zugfestigkeit of 860 MPa |
Chemical properties
Property | Value |
---|---|
Molybdän | 0.01 - 0.3 % Show Material materials with Molybdän of 0.01 - 0.3 % |
Niobium | 0.01 - 0.07 % Show Material materials with Niobium of 0.01 - 0.07 % |
Titan | 0.03 % Show Material materials with Titan of 0.03 % |
Vanadium | 0.02 - 0.2 % Show Material materials with Vanadium of 0.02 - 0.2 % |