Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Nickel Molybdenum Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 20.0 °C | 0 - 20 % Show Material materials with Dehnung A50 of 0 - 20 % | |
Flächenreduzierung | 20.0 °C | 0 - 35 % Show Material materials with Flächenreduzierung of 0 - 35 % | |
Poissonzahl | 20.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Molybdenum Steel |
Yield Strength Rp0.2, short transverse | 20.0 °C | 0 - 275 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 275 MPa | |
Zugfestigkeit | 20.0 °C | 0 - 484 MPa Show Material materials with Zugfestigkeit of 0 - 484 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 1/K | Typical for Nickel Molybdenum Steel 20-300°C |
Schmelzpunkt | 1529 °C Show Material materials with Schmelzpunkt of 1529 °C | Typical for Nickel Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.05 - 0.2 % Show Material materials with Kohlenstoff of 0.05 - 0.2 % |
Kupfer | 0 - 0.5 % Show Material materials with Kupfer of 0 - 0.5 % |
Mangan | 0.5 - 0.8 % Show Material materials with Mangan of 0.5 - 0.8 % |
Molybdän | 0.45 - 0.65 % Show Material materials with Molybdän of 0.45 - 0.65 % |
Phosphor | 0 - 0.04 % Show Material materials with Phosphor of 0 - 0.04 % |
Schwefel | 0 - 0.035 % Show Material materials with Schwefel of 0 - 0.035 % |
Silizium | 0 - 0.6 % Show Material materials with Silizium of 0 - 0.6 % |
Vanadium | 0 - 0.03 % Show Material materials with Vanadium of 0 - 0.03 % |
Wolfram | 0 - 0.1 % Show Material materials with Wolfram of 0 - 0.1 % |