Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Manganese Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 20.0 °C | 22 % Show Material materials with Dehnung A50 of 22 % | |
Elastizitätsmodul | 20.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Manganese Steel |
Flächenreduzierung | 20.0 °C | 35 % Show Material materials with Flächenreduzierung of 35 % | |
Poissonzahl | 20.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Manganese Steel |
Yield Strength Rp0.2, short transverse | 20.0 °C | 275 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 275 MPa | |
Zugfestigkeit | 20.0 °C | 485 MPa Show Material materials with Zugfestigkeit of 485 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.33E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.33E-5 1/K | Typical for Manganese Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Manganese Steel | |
Spezifische Wärmekapazität | 20.0 °C | 510 - 553 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 510 - 553 J/(kg·K) | Typical for Manganese Steel |
Wärmeleitfähigkeit | 20.0 °C | 14 - 16 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 - 16 W/(m·K) | Typical for Manganese Steel |
Chemical properties
Property | Value |
---|---|
Bor | 0.2 % Show Material materials with Bor of 0.2 % |
Kohlenstoff | 0.12 % Show Material materials with Kohlenstoff of 0.12 % |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % |
Mangan | 2.1 % Show Material materials with Mangan of 2.1 % |
Nickel | 0.02 % Show Material materials with Nickel of 0.02 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |