Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Dichte of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 20.0 °C | 0 - 18 % Show Material materials with Dehnung A50 of 0 - 18 % | |
Flächenreduzierung | 20.0 °C | 0 - 30 % Show Material materials with Flächenreduzierung of 0 - 30 % | |
Poissonzahl | 20.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Martensitic Stainless Steel |
Yield Strength Rp0.2, short transverse | 20.0 °C | 0 - 450 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 450 MPa | |
Zugfestigkeit | 20.0 °C | 0 - 620 MPa Show Material materials with Zugfestigkeit of 0 - 620 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Schmelzpunkt | 1375 - 1450 °C Show Material materials with Schmelzpunkt of 1375 - 1450 °C | Typical for Martensitic Stainless Steel | |
Wärmeleitfähigkeit | 20.0 °C | 14 - 31 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0 - 0.15 % Show Material materials with Kohlenstoff of 0 - 0.15 % |
Kupfer | 0 - 0.1 % Show Material materials with Kupfer of 0 - 0.1 % |
Mangan | 0 - 1 % Show Material materials with Mangan of 0 - 1 % |
Molybdän | 0.15 - 1 % Show Material materials with Molybdän of 0.15 - 1 % |
Nickel | 0 - 0.05 % Show Material materials with Nickel of 0 - 0.05 % |
Phosphor | 0 - 0.04 % Show Material materials with Phosphor of 0 - 0.04 % |
Schwefel | 0 - 0.035 % Show Material materials with Schwefel of 0 - 0.035 % |
Silizium | 0 - 0.65 % Show Material materials with Silizium of 0 - 0.65 % |