Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 21 % Show Material materials with Dehnung A50 of 21 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Low Carbon Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Low Carbon Steel |
Schubmodule | 23.0 °C | 82 GPa Show Material materials with Schubmodule of 82 GPa | Typical for Low Carbon Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 345 MPa Show Material materials with Streckgrenze Rp 0,2 of 345 MPa | |
Zugfestigkeit | 23.0 °C | 485 MPa Show Material materials with Zugfestigkeit of 485 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.32E-5 - 1.38E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32E-5 - 1.38E-5 1/K | Typical for Low Carbon Steel |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | Typical for Low Carbon Steel | |
Spezifische Wärmekapazität | 23.0 °C | 465 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 465 J/(kg·K) | Typical for Low Carbon Steel |
Wärmeleitfähigkeit | 23.0 °C | 25 - 93 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Magnetisch
Property | Value | Comment |
---|---|---|
Curie-Temperatur | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 - 0.04 % Show Material materials with Aluminium of 0.01 - 0.04 % |
Chrom | 0.45 - 0.7 % Show Material materials with Chrom of 0.45 - 0.7 % |
Kohlenstoff | 0.11 % Show Material materials with Kohlenstoff of 0.11 % |
Kupfer | 0.25 - 0.4 % Show Material materials with Kupfer of 0.25 - 0.4 % |
Mangan | 1.1 - 1.35 % Show Material materials with Mangan of 1.1 - 1.35 % |
Molybdän | 0.02 - 0.08 % Show Material materials with Molybdän of 0.02 - 0.08 % |
Nickel | 0.25 - 0.4 % Show Material materials with Nickel of 0.25 - 0.4 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 6E-3 % Show Material materials with Schwefel of 6E-3 % |
Silizium | 0.3 - 0.5 % Show Material materials with Silizium of 0.3 - 0.5 % |
Stickstoff | 0.02 % Show Material materials with Stickstoff of 0.02 % |
Vanadium | 0.04 - 0.08 % Show Material materials with Vanadium of 0.04 - 0.08 % |