Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 16 - 18 % Show Material materials with Dehnung A50 of 16 - 18 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 620 - 690 MPa Show Material materials with Streckgrenze Rp 0,2 of 620 - 690 MPa | |
Zugfestigkeit | 23.0 °C | 690 - 895 MPa Show Material materials with Zugfestigkeit of 690 - 895 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 - 0.05 % Show Material materials with Aluminium of 0.02 - 0.05 % |
Chrom | 0.4 - 0.65 % Show Material materials with Chrom of 0.4 - 0.65 % |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % |
Kupfer | 0.9 - 1.2 % Show Material materials with Kupfer of 0.9 - 1.2 % |
Mangan | 0.95 - 1.5 % Show Material materials with Mangan of 0.95 - 1.5 % |
Molybdän | 0.4 - 0.65 % Show Material materials with Molybdän of 0.4 - 0.65 % |
Nickel | 0.65 - 0.9 % Show Material materials with Nickel of 0.65 - 0.9 % |
Niobium | 0.01 - 0.03 % Show Material materials with Niobium of 0.01 - 0.03 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 6E-3 % Show Material materials with Schwefel of 6E-3 % |
Silizium | 0.15 - 0.35 % Show Material materials with Silizium of 0.15 - 0.35 % |
Stickstoff | 0.02 % Show Material materials with Stickstoff of 0.02 % |
Vanadium | 0.04 - 0.08 % Show Material materials with Vanadium of 0.04 - 0.08 % |