Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 15 - 18 % Show Material materials with Dehnung A50 of 15 - 18 % |
Elongation A200 | 23.0 °C | 12 % Show Material materials with Elongation A200 of 12 % |
Streckgrenze | 23.0 °C | 260 MPa Show Material materials with Streckgrenze of 260 MPa |
Zugfestigkeit | 23.0 °C | 450 - 585 MPa Show Material materials with Zugfestigkeit of 450 - 585 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 - 0.08 % Show Material materials with Aluminium of 0.02 - 0.08 % |
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % |
Kohlenstoff | 0.27 % Show Material materials with Kohlenstoff of 0.27 % |
Kupfer | 0.4 % Show Material materials with Kupfer of 0.4 % |
Mangan | 1.2 % Show Material materials with Mangan of 1.2 % |
Molybdän | 0.12 % Show Material materials with Molybdän of 0.12 % |
Nickel | 0.4 % Show Material materials with Nickel of 0.4 % |
Niobium | 0.02 % Show Material materials with Niobium of 0.02 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 0.3 % Show Material materials with Silizium of 0.3 % |
Titan | 0.03 % Show Material materials with Titan of 0.03 % |
Vanadium | 0.03 % Show Material materials with Vanadium of 0.03 % |