Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 0 - 20 % Show Material materials with Dehnung A50 of 0 - 20 % |
Kerbschlagenergie | 20.0 °C | 0 - 27 J Show Material materials with Kerbschlagenergie of 0 - 27 J |
Yield Strength Rp0.2, short transverse | 20.0 °C | 0 - 585 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 585 MPa |
Zugfestigkeit | 20.0 °C | 0 - 620 MPa Show Material materials with Zugfestigkeit of 0 - 620 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.6 - 0.9 % Show Material materials with Chrom of 0.6 - 0.9 % |
Kohlenstoff | 0 - 0.07 % Show Material materials with Kohlenstoff of 0 - 0.07 % |
Kupfer | 1 - 1.3 % Show Material materials with Kupfer of 1 - 1.3 % |
Mangan | 0.4 - 0.7 % Show Material materials with Mangan of 0.4 - 0.7 % |
Molybdän | 0.15 - 0.25 % Show Material materials with Molybdän of 0.15 - 0.25 % |
Nickel | 0.7 - 1 % Show Material materials with Nickel of 0.7 - 1 % |
Niobium | 0 - 0.02 % Show Material materials with Niobium of 0 - 0.02 % |
Phosphor | 0 - 0.03 % Show Material materials with Phosphor of 0 - 0.03 % |
Schwefel | 0 - 0.025 % Show Material materials with Schwefel of 0 - 0.025 % |
Silizium | 0 - 0.4 % Show Material materials with Silizium of 0 - 0.4 % |