Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 30 % Show Material materials with Dehnung A50 of 30 % |
Härte, Brinell | 20.0 °C | 217 [-] Show Material materials with Härte, Brinell of 217 [-] |
Härte, Rockwell B | 20.0 °C | 95 [-] Show Material materials with Härte, Rockwell B of 95 [-] |
Yield Strength Rp0.2, short transverse | 20.0 °C | 240 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 240 MPa |
Zugfestigkeit | 20.0 °C | 550 MPa Show Material materials with Zugfestigkeit of 550 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 19 - 21 % Show Material materials with Chrom of 19 - 21 % |
Kohlenstoff | 0.07 % Show Material materials with Kohlenstoff of 0.07 % |
Kupfer | 3 - 4 % Show Material materials with Kupfer of 3 - 4 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Molybdän | 2 - 3 % Show Material materials with Molybdän of 2 - 3 % |
Nickel | 32 - 38 % Show Material materials with Nickel of 32 - 38 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |