Austenitischer rostfreier Stahl
Alloy 24 / 1.4565 Solution annealed and quenchedGeliefert von:
Hempel Special MetalsDuplex rostfreier Stahl
Sandvik SAF 2205™ Solution AnnealedGeliefert von:
Alleima (formerly Sandvik Materials Technology)Duplex rostfreier Stahl
Sandvik SAF 2507® Solution AnnealedGeliefert von:
Alleima (formerly Sandvik Materials Technology)Duplex rostfreier Stahl
Sandvik SAF 2205™ Cold WorkedGeliefert von:
Alleima (formerly Sandvik Materials Technology)Duplex rostfreier Stahl
Sandvik SAF 2507® Cold WorkedGeliefert von:
Alleima (formerly Sandvik Materials Technology)Nickel Chromium Iron Alloy
Sandvik 2RK65™Geliefert von:
Alleima (formerly Sandvik Materials Technology)Duplex rostfreier Stahl
Sandvik SAF 2906™Geliefert von:
Alleima (formerly Sandvik Materials Technology)Duplex rostfreier Stahl
S32550 / AMAZON 256 Duplex Stainless SteelAustenitischer rostfreier Stahl
ASTM A240 Grade 304LN Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade 316L Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade 316LN Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade 321 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade 304 Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade 304N Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade 310Cb Heat-TreatedAustenitischer rostfreier Stahl
ASTM A240 Grade 310H Heat-Treated