Mechanisch
Chemical properties
Property | Value |
---|---|
Chrom | 15.5 - 17.5 % Show Material materials with Chrom of 15.5 - 17.5 % |
Eisen | 4.5 - 7.5 % Show Material materials with Eisen of 4.5 - 7.5 % |
Kohlenstoff | 0.12 % Show Material materials with Kohlenstoff of 0.12 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 16 - 18 % Show Material materials with Molybdän of 16 - 18 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Vanadium | 0.2 - 0.4 % Show Material materials with Vanadium of 0.2 - 0.4 % |
Wolfram | 3.75 - 5.25 % Show Material materials with Wolfram of 3.75 - 5.25 % |