Mechanisch
Chemical properties
Property | Value |
---|---|
Chrom | 17 - 20 % Show Material materials with Chrom of 17 - 20 % |
Eisen | 3 % Show Material materials with Eisen of 3 % |
Kohlenstoff | 0.07 % Show Material materials with Kohlenstoff of 0.07 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 17 - 20 % Show Material materials with Molybdän of 17 - 20 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |