Mechanisch
Chemical properties
Property | Value |
---|---|
Chrom | 20 - 23 % Show Material materials with Chrom of 20 - 23 % |
Eisen | 5 % Show Material materials with Eisen of 5 % |
Kohlenstoff | 0.06 % Show Material materials with Kohlenstoff of 0.06 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 8 - 10 % Show Material materials with Molybdän of 8 - 10 % |
Niobium | 3.15 - 4.5 % Show Material materials with Niobium of 3.15 - 4.5 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |