Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 11 % Show Material materials with Dehnung A50 of 11 % | |
Dehnung A50, transversal | 23.0 °C | 11 % Show Material materials with Dehnung A50, transversal of 11 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 50 % Show Material materials with Flächenreduzierung of 50 % | |
Flächenreduzierung, transversal | 23.0 °C | 45 % Show Material materials with Flächenreduzierung, transversal of 45 % | |
Hardness, Brinell, trans | 23.0 °C | 380 [-] Show Material materials with Hardness, Brinell, trans of 380 [-] | |
Härte, Brinell | 23.0 °C | 380 [-] Show Material materials with Härte, Brinell of 380 [-] | |
Härte, Rockwell C | 23.0 °C | 41 [-] Show Material materials with Härte, Rockwell C of 41 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 1210 MPa Show Material materials with Streckgrenze Rp 0,2 of 1210 MPa | |
Streckgrenze Rp 0,2, transversal | 23.0 °C | 1210 MPa Show Material materials with Streckgrenze Rp 0,2, transversal of 1210 MPa | |
Zugfestigkeit | 23.0 °C | 1280 MPa Show Material materials with Zugfestigkeit of 1280 MPa | |
Zugfestigkeit, transversal | 23.0 °C | 1280 MPa Show Material materials with Zugfestigkeit, transversal of 1280 MPa |