Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 10 % Show Material materials with Dehnung A50 of 10 % | |
Dehnung A50, transversal | 23.0 °C | 8 % Show Material materials with Dehnung A50, transversal of 8 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 45 % Show Material materials with Flächenreduzierung of 45 % | |
Flächenreduzierung, transversal | 23.0 °C | 35 % Show Material materials with Flächenreduzierung, transversal of 35 % | |
Hardness, Brinell, trans | 23.0 °C | 444 [-] Show Material materials with Hardness, Brinell, trans of 444 [-] | |
Härte, Brinell | 23.0 °C | 444 [-] Show Material materials with Härte, Brinell of 444 [-] | |
Härte, Rockwell C | 23.0 °C | 47 [-] Show Material materials with Härte, Rockwell C of 47 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 1515 MPa Show Material materials with Streckgrenze Rp 0,2 of 1515 MPa | |
Streckgrenze Rp 0,2, transversal | 23.0 °C | 1515 MPa Show Material materials with Streckgrenze Rp 0,2, transversal of 1515 MPa | |
Zugfestigkeit | 23.0 °C | 1655 MPa Show Material materials with Zugfestigkeit of 1655 MPa | |
Zugfestigkeit, transversal | 23.0 °C | 1655 MPa Show Material materials with Zugfestigkeit, transversal of 1655 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 11 - 12.5 % Show Material materials with Chrom of 11 - 12.5 % |
Kohlenstoff | 0.02 % Show Material materials with Kohlenstoff of 0.02 % |
Mangan | 0.25 % Show Material materials with Mangan of 0.25 % |
Molybdän | 0.75 - 1.25 % Show Material materials with Molybdän of 0.75 - 1.25 % |
Nickel | 10.75 - 11.25 % Show Material materials with Nickel of 10.75 - 11.25 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.25 % Show Material materials with Silizium of 0.25 % |
Titan | 1.5 - 1.8 % Show Material materials with Titan of 1.5 - 1.8 % |