Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Manganese Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 20 % Show Material materials with Dehnung A50 of 20 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Manganese Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Manganese Steel |
Streckgrenze | 23.0 °C | 300 MPa Show Material materials with Streckgrenze of 300 MPa | |
Zugfestigkeit | 23.0 °C | 390 MPa Show Material materials with Zugfestigkeit of 390 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.33E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.33E-5 1/K | Typical for Manganese Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Manganese Steel | |
Spezifische Wärmekapazität | 23.0 °C | 510 - 553 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 510 - 553 J/(kg·K) | Typical for Manganese Steel |
Wärmeleitfähigkeit | 23.0 °C | 14 - 16 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 - 16 W/(m·K) | Typical for Manganese Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 0.15 % Show Material materials with Chrom of 0.15 % |
Kohlenstoff | 0.12 % Show Material materials with Kohlenstoff of 0.12 % |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Molybdän | 0.06 % Show Material materials with Molybdän of 0.06 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Niobium | 8E-3 % Show Material materials with Niobium of 8E-3 % |
Phosphor | 0.12 % Show Material materials with Phosphor of 0.12 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Titan | 0.03 % Show Material materials with Titan of 0.03 % |
Vanadium | 8E-3 % Show Material materials with Vanadium of 8E-3 % |