Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 25 % Show Material materials with Dehnung A50 of 25 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Härte, Rockwell B | 23.0 °C | 100 [-] Show Material materials with Härte, Rockwell B of 100 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 450 MPa Show Material materials with Streckgrenze of 450 MPa | |
Zugfestigkeit | 23.0 °C | 1035 MPa Show Material materials with Zugfestigkeit of 1035 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.75 - 1.5 % Show Material materials with Aluminium of 0.75 - 1.5 % |
Chrom | 14 - 16 % Show Material materials with Chrom of 14 - 16 % |
Kohlenstoff | 0.09 % Show Material materials with Kohlenstoff of 0.09 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 2 - 3 % Show Material materials with Molybdän of 2 - 3 % |
Nickel | 6.5 - 7.7 % Show Material materials with Nickel of 6.5 - 7.7 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |