Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 8 - 12 % Show Material materials with Dehnung A50 of 8 - 12 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Härte, Rockwell C | 23.0 °C | 30 [-] Show Material materials with Härte, Rockwell C of 30 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 585 - 620 MPa Show Material materials with Streckgrenze of 585 - 620 MPa | |
Zugfestigkeit | 23.0 °C | 1380 MPa Show Material materials with Zugfestigkeit of 1380 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 16 - 17 % Show Material materials with Chrom of 16 - 17 % |
Kohlenstoff | 0.07 - 0.11 % Show Material materials with Kohlenstoff of 0.07 - 0.11 % |
Mangan | 0.5 - 1.25 % Show Material materials with Mangan of 0.5 - 1.25 % |
Molybdän | 2.5 - 3.2 % Show Material materials with Molybdän of 2.5 - 3.2 % |
Nickel | 4 - 5 % Show Material materials with Nickel of 4 - 5 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |