Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 25 - 35 % Show Material materials with Dehnung A50 of 25 - 35 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 260 - 270 MPa Show Material materials with Streckgrenze of 260 - 270 MPa | |
Zugfestigkeit | 23.0 °C | 600 - 650 MPa Show Material materials with Zugfestigkeit of 600 - 650 MPa |
Chemical properties
Property | Value |
---|---|
Cerium | 0.03 - 0.08 % Show Material materials with Cerium of 0.03 - 0.08 % |
Chrom | 24 - 26 % Show Material materials with Chrom of 24 - 26 % |
Kohlenstoff | 0.04 - 0.08 % Show Material materials with Kohlenstoff of 0.04 - 0.08 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Nickel | 34 - 36 % Show Material materials with Nickel of 34 - 36 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1.2 - 2 % Show Material materials with Silizium of 1.2 - 2 % |
Stickstoff | 0.12 - 0.18 % Show Material materials with Stickstoff of 0.12 - 0.18 % |