Mechanisch
Chemical properties
Property | Value |
---|---|
Chrom | 19 - 21 % Show Material materials with Chrom of 19 - 21 % |
Kohlenstoff | 0.02 % Show Material materials with Kohlenstoff of 0.02 % |
Kupfer | 0.5 - 1.5 % Show Material materials with Kupfer of 0.5 - 1.5 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Molybdän | 6 - 7 % Show Material materials with Molybdän of 6 - 7 % |
Nickel | 24 - 26 % Show Material materials with Nickel of 24 - 26 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Stickstoff | 0.15 - 0.25 % Show Material materials with Stickstoff of 0.15 - 0.25 % |