Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 30 % Show Material materials with Dehnung A50 of 30 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 40 % Show Material materials with Flächenreduzierung of 40 % | |
Kerbschlagenergie | 23.0 °C | 20 J Show Material materials with Kerbschlagenergie of 20 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 360 MPa Show Material materials with Streckgrenze Rp 0,2 of 360 MPa | |
Zugfestigkeit | 23.0 °C | 455 - 630 MPa Show Material materials with Zugfestigkeit of 455 - 630 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % |
Kohlenstoff | 0.22 % Show Material materials with Kohlenstoff of 0.22 % |
Kupfer | 0.4 % Show Material materials with Kupfer of 0.4 % |
Mangan | 1.15 - 1.5 % Show Material materials with Mangan of 1.15 - 1.5 % |
Molybdän | 0.12 % Show Material materials with Molybdän of 0.12 % |
Nickel | 0.4 % Show Material materials with Nickel of 0.4 % |
Niobium | 0.02 % Show Material materials with Niobium of 0.02 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.15 - 0.3 % Show Material materials with Silizium of 0.15 - 0.3 % |
Stickstoff | 0.01 - 0.03 % Show Material materials with Stickstoff of 0.01 - 0.03 % |
Vanadium | 0.04 - 0.11 % Show Material materials with Vanadium of 0.04 - 0.11 % |