Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 18 - 28 % Show Material materials with Dehnung A50 of 18 - 28 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Kerbschlagenergie | 23.0 °C | 17.6 J Show Material materials with Kerbschlagenergie of 17.6 J | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 315 MPa Show Material materials with Streckgrenze of 315 MPa | |
Zugfestigkeit | 23.0 °C | 435 - 610 MPa Show Material materials with Zugfestigkeit of 435 - 610 MPa |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % |
Kupfer | 0.75 - 1.25 % Show Material materials with Kupfer of 0.75 - 1.25 % |
Mangan | 0.4 - 1.06 % Show Material materials with Mangan of 0.4 - 1.06 % |
Nickel | 1.6 - 2.24 % Show Material materials with Nickel of 1.6 - 2.24 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |