Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 30 % Show Material materials with Dehnung A50 of 30 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 50 % Show Material materials with Flächenreduzierung of 50 % | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 205 MPa Show Material materials with Streckgrenze Rp 0,2 of 205 MPa | |
Zugfestigkeit | 23.0 °C | 550 MPa Show Material materials with Zugfestigkeit of 550 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 7 - 9 % Show Material materials with Chrom of 7 - 9 % |
Kohlenstoff | 0.1 - 0.2 % Show Material materials with Kohlenstoff of 0.1 - 0.2 % |
Mangan | 0.5 - 0.8 % Show Material materials with Mangan of 0.5 - 0.8 % |
Nickel | 19 - 22 % Show Material materials with Nickel of 19 - 22 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 - 1.4 % Show Material materials with Silizium of 1 - 1.4 % |