Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 15 % Show Material materials with Dehnung A50 of 15 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 30 % Show Material materials with Flächenreduzierung of 30 % | |
Härte, Brinell | 23.0 °C | 310 [-] Show Material materials with Härte, Brinell of 310 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 550 MPa Show Material materials with Streckgrenze Rp 0,2 of 550 MPa | |
Zugfestigkeit | 23.0 °C | 800 MPa Show Material materials with Zugfestigkeit of 800 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 24 - 26 % Show Material materials with Chrom of 24 - 26 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Mangan | 1.2 % Show Material materials with Mangan of 1.2 % |
Molybdän | 3 - 5 % Show Material materials with Molybdän of 3 - 5 % |
Nickel | 6 - 8 % Show Material materials with Nickel of 6 - 8 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 0.8 % Show Material materials with Silizium of 0.8 % |