Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.9 - 8.2 g/cm³ Show Material materials with Dichte of 7.9 - 8.2 g/cm³ | Typical for Austenitic Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 20.0 °C | 35 % Show Material materials with Dehnung A50 of 35 % | |
Elastizitätsmodul | 20.0 °C | 195 GPa Show Material materials with Elastizitätsmodul of 195 GPa | Typical for Austenitic Stainless Steel |
Flächenreduzierung | 20.0 °C | 55 % Show Material materials with Flächenreduzierung of 55 % | |
Härte, Brinell | 20.0 °C | 271 [-] Show Material materials with Härte, Brinell of 271 [-] | |
Härte, Rockwell C | 20.0 °C | 28 [-] Show Material materials with Härte, Rockwell C of 28 [-] | |
Poissonzahl | 20.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Yield Strength Rp0.2, short transverse | 20.0 °C | 380 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 380 MPa | |
Zugfestigkeit | 20.0 °C | 690 MPa Show Material materials with Zugfestigkeit of 690 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.7E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 - 1.9E-5 1/K | Typical for Austenitic Stainless Steel |
Schmelzpunkt | 1375 - 1450 °C Show Material materials with Schmelzpunkt of 1375 - 1450 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 20.0 °C | 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Wärmeleitfähigkeit | 20.0 °C | 11 - 21 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 20.0 °C | 8.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 20.5 - 23.5 % Show Material materials with Chrom of 20.5 - 23.5 % |
Kohlenstoff | 0.06 % Show Material materials with Kohlenstoff of 0.06 % |
Mangan | 4 - 6 % Show Material materials with Mangan of 4 - 6 % |
Molybdän | 1.5 - 3 % Show Material materials with Molybdän of 1.5 - 3 % |
Nickel | 11.5 - 13.5 % Show Material materials with Nickel of 11.5 - 13.5 % |
Niobium | 0.1 - 0.3 % Show Material materials with Niobium of 0.1 - 0.3 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Stickstoff | 0.2 - 0.4 % Show Material materials with Stickstoff of 0.2 - 0.4 % |
Vanadium | 0.1 - 0.3 % Show Material materials with Vanadium of 0.1 - 0.3 % |