Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.9 - 8.2 g/cm³ Show Material materials with Dichte of 7.9 - 8.2 g/cm³ | Typical for Austenitic Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 20 % Show Material materials with Dehnung A50 of 20 % | |
Elastizitätsmodul | 23.0 °C | 195 GPa Show Material materials with Elastizitätsmodul of 195 GPa | Typical for Austenitic Stainless Steel |
Härte, Brinell | 23.0 °C | 190 - 250 [-] Show Material materials with Härte, Brinell of 190 - 250 [-] | |
Härte, Rockwell B | 23.0 °C | 90 [-] Show Material materials with Härte, Rockwell B of 90 [-] | |
Härte, Rockwell C | 23.0 °C | 25 [-] Show Material materials with Härte, Rockwell C of 25 [-] | |
Härte, Vickers | 23.0 °C | 196 - 265 [-] Show Material materials with Härte, Vickers of 196 - 265 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Streckgrenze | 23.0 °C | 450 MPa Show Material materials with Streckgrenze of 450 MPa | |
Zugfestigkeit | 23.0 °C | 620 MPa Show Material materials with Zugfestigkeit of 620 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.7E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 - 1.9E-5 1/K | Typical for Austenitic Stainless Steel |
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 8.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Bor | 1E-3 % Show Material materials with Bor of 1E-3 % |
Chrom | 10 - 11 % Show Material materials with Chrom of 10 - 11 % |
Kohlenstoff | 0.08 - 0.13 % Show Material materials with Kohlenstoff of 0.08 - 0.13 % |
Mangan | 0.2 - 0.5 % Show Material materials with Mangan of 0.2 - 0.5 % |
Molybdän | 0.4 - 0.6 % Show Material materials with Molybdän of 0.4 - 0.6 % |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % |
Niobium | 0.02 - 0.06 % Show Material materials with Niobium of 0.02 - 0.06 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 5E-3 % Show Material materials with Schwefel of 5E-3 % |
Silizium | 0.15 - 0.45 % Show Material materials with Silizium of 0.15 - 0.45 % |
Stickstoff | 0.03 - 0.07 % Show Material materials with Stickstoff of 0.03 - 0.07 % |
Vanadium | 0.18 - 0.25 % Show Material materials with Vanadium of 0.18 - 0.25 % |