Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 20 % Show Material materials with Dehnung A50 of 20 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Härte, Brinell | 23.0 °C | 250 [-] Show Material materials with Härte, Brinell of 250 [-] | |
Härte, Rockwell C | 23.0 °C | 25 [-] Show Material materials with Härte, Rockwell C of 25 [-] | |
Härte, Vickers | 23.0 °C | 265 [-] Show Material materials with Härte, Vickers of 265 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 440 MPa Show Material materials with Streckgrenze of 440 MPa | |
Zugfestigkeit | 23.0 °C | 620 MPa Show Material materials with Zugfestigkeit of 620 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Bor | 3E-4 - 6E-3 % Show Material materials with Bor of 3E-4 - 6E-3 % |
Chrom | 8.5 - 9.5 % Show Material materials with Chrom of 8.5 - 9.5 % |
Kohlenstoff | 0.09 - 0.13 % Show Material materials with Kohlenstoff of 0.09 - 0.13 % |
Mangan | 0.3 - 0.6 % Show Material materials with Mangan of 0.3 - 0.6 % |
Molybdän | 0.9 - 1.1 % Show Material materials with Molybdän of 0.9 - 1.1 % |
Nickel | 0.4 % Show Material materials with Nickel of 0.4 % |
Niobium | 0.06 - 0.1 % Show Material materials with Niobium of 0.06 - 0.1 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.1 - 0.5 % Show Material materials with Silizium of 0.1 - 0.5 % |
Stickstoff | 0.04 - 0.09 % Show Material materials with Stickstoff of 0.04 - 0.09 % |
Vanadium | 0.18 - 0.25 % Show Material materials with Vanadium of 0.18 - 0.25 % |
Wolfram | 0.9 - 1.1 % Show Material materials with Wolfram of 0.9 - 1.1 % |