Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 20 % Show Material materials with Dehnung A50 of 20 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Härte, Brinell | 23.0 °C | 207 [-] Show Material materials with Härte, Brinell of 207 [-] | |
Härte, Rockwell B | 23.0 °C | 95 [-] Show Material materials with Härte, Rockwell B of 95 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 275 MPa Show Material materials with Streckgrenze of 275 MPa | |
Zugfestigkeit | 23.0 °C | 485 MPa Show Material materials with Zugfestigkeit of 485 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 18 - 23 % Show Material materials with Chrom of 18 - 23 % |
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % |
Kupfer | 0.9 - 1.25 % Show Material materials with Kupfer of 0.9 - 1.25 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 0.75 % Show Material materials with Nickel of 0.75 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |