Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.6 - 7.8 g/cm³ Show Material materials with Dichte of 7.6 - 7.8 g/cm³ | Typical for Ferritic Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 20 % Show Material materials with Dehnung A50 of 20 % | |
Elastizitätsmodul | 23.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | Typical for Ferritic Stainless Steel |
Härte, Brinell | 23.0 °C | 241 [-] Show Material materials with Härte, Brinell of 241 [-] | |
Härte, Rockwell B | 23.0 °C | 100 [-] Show Material materials with Härte, Rockwell B of 100 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Ferritic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Ferritic Stainless Steel |
Streckgrenze | 23.0 °C | 275 MPa Show Material materials with Streckgrenze of 275 MPa | |
Zugfestigkeit | 23.0 °C | 450 MPa Show Material materials with Zugfestigkeit of 450 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 9.3E-6 - 1.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.3E-6 - 1.2E-5 1/K | Typical for Ferritic Stainless Steel |
Schmelzpunkt | 1425 - 1530 °C Show Material materials with Schmelzpunkt of 1425 - 1530 °C | Typical for Ferritic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 420 - 586 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 420 - 586 J/(kg·K) | Typical for Ferritic Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 11 - 22 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 11 - 22 W/(m·K) | Typical for Ferritic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 6E-7 - 7.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 6E-7 - 7.5E-7 Ω·m | Typical for Ferritic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 25 - 27.5 % Show Material materials with Chrom of 25 - 27.5 % |
Kohlenstoff | 0.01 % Show Material materials with Kohlenstoff of 0.01 % |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % |
Mangan | 0.4 % Show Material materials with Mangan of 0.4 % |
Molybdän | 0.75 - 1.5 % Show Material materials with Molybdän of 0.75 - 1.5 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Niobium | 0.05 - 0.2 % Show Material materials with Niobium of 0.05 - 0.2 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % |
Stickstoff | 0.02 % Show Material materials with Stickstoff of 0.02 % |