Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 40 % Show Material materials with Dehnung A50 of 40 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 50 % Show Material materials with Flächenreduzierung of 50 % | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 205 MPa Show Material materials with Streckgrenze Rp 0,2 of 205 MPa | |
Zugfestigkeit | 23.0 °C | 515 MPa Show Material materials with Zugfestigkeit of 515 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 17 - 19 % Show Material materials with Chrom of 17 - 19 % |
Kohlenstoff | 0.15 % Show Material materials with Kohlenstoff of 0.15 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Nickel | 8 - 10 % Show Material materials with Nickel of 8 - 10 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 2 - 3 % Show Material materials with Silizium of 2 - 3 % |
Stickstoff | 0.1 % Show Material materials with Stickstoff of 0.1 % |