Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Nickel Molybdenum Steel |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 18.5 % Show Material materials with Dehnung of 18.5 % | Predicted Value, A80 | |||
19 % Show Material materials with Dehnung of 19 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate | A200 | |
19.2 % Show Material materials with Dehnung of 19.2 % | Predicted Value, Transverse | ||||
19.7 % Show Material materials with Dehnung of 19.7 % | Predicted Value, A80 Transverse | ||||
22 % Show Material materials with Dehnung of 22 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate | A50 | |
25.9 % Show Material materials with Dehnung of 25.9 % | Predicted Value | ||||
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Molybdenum Steel | |||
Flächenreduzierung | 41.5 % Show Material materials with Flächenreduzierung of 41.5 % | Predicted Value | |||
44.3 % Show Material materials with Flächenreduzierung of 44.3 % | Predicted Value, Transverse | ||||
Poissonzahl | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Molybdenum Steel | |||
Scherfestigkeit | 607.8 MPa Show Material materials with Scherfestigkeit of 607.8 MPa | Predicted Value | |||
Schubmodule | 79.4 GPa Show Material materials with Schubmodule of 79.4 GPa | Predicted Value | |||
Streckgrenze | 240 MPa Show Material materials with Streckgrenze of 240 MPa | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate | |
261.3 MPa Show Material materials with Streckgrenze of 261.3 MPa | Predicted Value, RP1 | ||||
317.1 MPa Show Material materials with Streckgrenze of 317.1 MPa | Predicted Value, RP1 Transverse | ||||
324.6 MPa Show Material materials with Streckgrenze of 324.6 MPa | Predicted Value, RP05 | ||||
330.9 MPa Show Material materials with Streckgrenze of 330.9 MPa | Predicted Value, Transverse | ||||
347.6 MPa Show Material materials with Streckgrenze of 347.6 MPa | Predicted Value, RP02 | ||||
437.5 MPa Show Material materials with Streckgrenze of 437.5 MPa | Predicted Value, RP002 | ||||
469.7 MPa Show Material materials with Streckgrenze of 469.7 MPa | Predicted Value, RP02 Transverse | ||||
Zugfestigkeit | 415 - 585 MPa Show Material materials with Zugfestigkeit of 415 - 585 MPa | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 9e-06 - 1.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9e-06 - 1.3e-05 1/K | Typical for Nickel Molybdenum Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Nickel Molybdenum Steel |
Spezifische Wärmekapazität | 335 - 481 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 335 - 481 J/(kg·K) | Typical for Nickel Molybdenum Steel |
Wärmeleitfähigkeit | 44 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 44 W/(m·K) | Typical for Nickel Molybdenum Steel |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 1 - 1.5 % Show Material materials with Chrom of 1 - 1.5 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Kohlenstoff | 0.05 - 0.17 % Show Material materials with Kohlenstoff of 0.05 - 0.17 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Mangan | 0.4 - 0.65 % Show Material materials with Mangan of 0.4 - 0.65 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Molybdän | 0.45 - 0.65 % Show Material materials with Molybdän of 0.45 - 0.65 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Silizium | 0.5 - 0.8 % Show Material materials with Silizium of 0.5 - 0.8 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |