Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 16.6 % Show Material materials with Dehnung of 16.6 % | Predicted Value, A200 | |||
18 % Show Material materials with Dehnung of 18 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate | A50 | |
18.8 % Show Material materials with Dehnung of 18.8 % | Predicted Value, Transverse | ||||
20 % Show Material materials with Dehnung of 20 % | Predicted Value, A80 Transverse | ||||
22.2 % Show Material materials with Dehnung of 22.2 % | Predicted Value, A80 | ||||
25.9 % Show Material materials with Dehnung of 25.9 % | Predicted Value | ||||
Elastizitätsmodul | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel | |||
Flächenreduzierung | 43.3 % Show Material materials with Flächenreduzierung of 43.3 % | Predicted Value, Transverse | |||
45 % Show Material materials with Flächenreduzierung of 45 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate | ||
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel | |||
Scherfestigkeit | 628.2 MPa Show Material materials with Scherfestigkeit of 628.2 MPa | Predicted Value | |||
Schubmodule | 79.3 GPa Show Material materials with Schubmodule of 79.3 GPa | Predicted Value | |||
Streckgrenze | 205 MPa Show Material materials with Streckgrenze of 205 MPa | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate | |
254.7 MPa Show Material materials with Streckgrenze of 254.7 MPa | Predicted Value, RP1 | ||||
310.6 MPa Show Material materials with Streckgrenze of 310.6 MPa | Predicted Value, Transverse | ||||
320.5 MPa Show Material materials with Streckgrenze of 320.5 MPa | Predicted Value, RP1 Transverse | ||||
326.6 MPa Show Material materials with Streckgrenze of 326.6 MPa | Predicted Value, RP05 | ||||
334.7 MPa Show Material materials with Streckgrenze of 334.7 MPa | Predicted Value, RP02 | ||||
438 MPa Show Material materials with Streckgrenze of 438 MPa | Predicted Value, RP02 Transverse | ||||
452.7 MPa Show Material materials with Streckgrenze of 452.7 MPa | Predicted Value, RP002 | ||||
Zugfestigkeit | 415 - 585 MPa Show Material materials with Zugfestigkeit of 415 - 585 MPa | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 11.99 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 11.99 1/K | Predicted Value |
Spezifische Wärmekapazität | 458.9 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 458.9 J/(kg·K) | Predicted Value |
Wärmeleitfähigkeit | 36.62 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36.62 W/(m·K) | Predicted Value |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 2 - 2.5 % Show Material materials with Chrom of 2 - 2.5 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Kohlenstoff | 0.05 - 0.15 % Show Material materials with Kohlenstoff of 0.05 - 0.15 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Mangan | 0.3 - 0.6 % Show Material materials with Mangan of 0.3 - 0.6 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Molybdän | 0.9 - 1.1 % Show Material materials with Molybdän of 0.9 - 1.1 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |