Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 0 - 18 % Show Material materials with Dehnung A50 of 0 - 18 % |
Flächenreduzierung | 20.0 °C | 0 - 45 % Show Material materials with Flächenreduzierung of 0 - 45 % |
Streckgrenze | 20.0 °C | 0 - 205 MPa Show Material materials with Streckgrenze of 0 - 205 MPa |
Zugfestigkeit | 20.0 °C | 415 - 585 MPa Show Material materials with Zugfestigkeit of 415 - 585 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 4 - 6 % Show Material materials with Chrom of 4 - 6 % |
Kohlenstoff | 0 - 0.15 % Show Material materials with Kohlenstoff of 0 - 0.15 % |
Mangan | 0.3 - 0.6 % Show Material materials with Mangan of 0.3 - 0.6 % |
Molybdän | 0.45 - 0.65 % Show Material materials with Molybdän of 0.45 - 0.65 % |
Phosphor | 0 - 0.03 % Show Material materials with Phosphor of 0 - 0.03 % |
Schwefel | 0 - 0.025 % Show Material materials with Schwefel of 0 - 0.025 % |
Silizium | 0 - 0.5 % Show Material materials with Silizium of 0 - 0.5 % |