Mechanisch
Chemical properties
Property | Value |
---|---|
Chrom | 20 - 22 % Show Material materials with Chrom of 20 - 22 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Mangan | 2 % Show Material materials with Mangan of 2 % |
Molybdän | 6 - 7 % Show Material materials with Molybdän of 6 - 7 % |
Nickel | 23.5 - 25.5 % Show Material materials with Nickel of 23.5 - 25.5 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Stickstoff | 0.18 - 0.25 % Show Material materials with Stickstoff of 0.18 - 0.25 % |